Types | Maintenance / Cleaning | Cleaning Frequency |
Austenitic stainless steel. General requirement to ASTM A 1016: 2002 or to BS 1449: Part 2 or BS 970: Part 1, grade 316, or BS EN 10088-2, grade 1.4401. Terne coated to BS 6582. [1] | Inspection:
Annual inspection and maintenance in accordance with BS 5427: Part 1, Table 9. [1] Renewal of side/ end lap seal as necessary. [1] Cleaning: Regular cleaning with non-alkaline detergent The preferred solvent is one that does not contain chlorine, such as acetone, methyl alcohol, and mineral spirits. [13] |
Polluted/ marine areas/ heavy industrial: every 3 months (4x/ year)
Other areas: every 6 month (2x/ year) |
Austenitic stainless steel. General requirement to ASTM A 1016: 2002 or to BS 1449: Part 2 or BS 970: Part 1, grade 316, or BS EN 10088-2, grade 1.4401.[1] | ||
Austenitic stainless steel. General requirement to ASTM A 1016: 2002 or to BS 1449: Part 2 or BS 970: Part 1, grade 304, or BS EN 10088-2, grade 1.4301. Terne coated to BS 6582.[1] | ||
Austenitic stainless steel. General requirement to ASTM A 1016: 2002 orto BS 1449: Part 2 or BS 970: Part 1, grade 304, or BS EN 10088-2, grade 1.4301. Factory applied organic coating, 25-50 microns nominal thickness.[1] | ||
Austenitic stainless steel. General requirement to ASTM A 1016: 2002 or to BS 1449: Part 2 or BS 970: Part 1, grade 304, or BS EN 10088-2, grade 1.4301 | ||
Ferritic stainless steel. General requirement to ASTM A 1016: 2002 or to BS 1449: Part 2 or BS 970: Part 1, grade 430 or 434, or BS EN 10088-2, grade 1.4000 or 1.4113. Factory applied organic coating, 25-50 microns nominal thickness | ||
Stainless steel, not to ASTM A 1016: 2002 or BS 1449: Part 2/ BS EN 10088-2, or less than above specifications. | None | None |