Fibre Cement Slate

Navigation

Types and Durability

Description

Fibre Cement Slates

Expected Lifespan

(Years)

Adjustment Factors
Fibre reinforced cement based slates*. Complying with requirements of ASTM C 1530-02 or BS 4624. 75-100 1st stage adjustment factor:

In industrial areas (heavy polluted): -15% years

In urban areas: -10% years

In suburban areas: -0% years

2nd stage adjustment factor:

Within 20m from express way: -20% years

Within 20m from major arterial road: -10% years

Within 20m from light traffic road: – 5% years

Test certificate from approved local testing authority : +15% years

Asbestos cement slate complying with requirements of ASTM C 1530-02 or BS EN 492. (previously BS 690 Part 4). Colour may be natural or achieved by using suitable pigments in the manufacture. 25
Non-Asbestos cement slate complying with requirements of ASTM C 1530-02 or BS EN 492. 40-75
Asbestos or fibre reinforced cement slates not complying with the requirements of BS EN 492 (previously BS 690 Part 4), or uncoated non-asbestos fibre reinforced slates. < 10 None

*Manufactured using Portland cement, pigments and other constituent.

Combination of adjustment factor (1st stage and 2nd stage) should be added to obtain the durability values. Refer to durability calculator